Level Up Your 3D Prints.
Price your prints right, pick the best gear, and fix every print problem. Everything makers need, in one place.
Join the official Tech You Unbox WhatsApp group
New Studio tools and updates first, help with the website and Studio, and support straight from the Tech You Unbox team.
One website, three superpowers
Accurate Print Pricing
Add up filament, electricity, machine wear and labour to get the real cost. Then create a professional GST invoice in one click.
Open calculatorBest Gear Guides
From affordable, reliable printers to premium filament: tested and honest buying guides.
Read guidesPrinter Doctor
Print failed? Find your problem among 22 common issues and get a step-by-step fix.
Fix a problemNew Gear Guides
3D Printing Gear Guides
Honest buying guides for printers, filament and accessories. Search or scroll to browse.
3D Print Cost Calculator
Enter all values for ONE piece. The total is calculated automatically with quantity and GST.
Printer & Job
Pick a printer and its watts and maintenance cost are filled in automatically.
Electricity & Machine
Profit & GST
Invoice Details
Live Estimate
Only for you| # | Item / Description | Qty | Rate | Amount |
|---|---|---|---|---|
| 1 |
Print failed? Fix it here.
The 22 most common 3D printing problems. Search for your issue or pick a category, open a card and follow the step-by-step fix.
🧲
Print not sticking to the bed (Bed Adhesion)
The first layer lifts, the print moves, or it comes loose halfway through.
Print not sticking to the bed (Bed Adhesion)
The first layer lifts, the print moves, or it comes loose halfway through.
How to fix
- Clean the bed with 99% IPA (isopropyl alcohol). Finger oil is the biggest enemy.
- Check the Z-offset: bring the nozzle slightly closer to the bed (paper test or live-adjust).
- Raise the bed temperature by 5°C. Typical values: PLA 55-65°C, PETG 70-80°C.
- Keep the first layer speed at 20-30 mm/s and turn the cooling fan off for the first layer.
- Add a brim (5-8 mm) on models with a small footprint; use a glue stick if needed.
📐
Corners curling up (Warping)
The corners of the model lift off the bed, especially with ABS, ASA and Nylon.
Corners curling up (Warping)
The corners of the model lift off the bed, especially with ABS, ASA and Nylon.
How to fix
- Plastic shrinks as it cools, so keep the heat in: use an enclosure or a draft shield.
- Add an 8-10 mm brim or 'mouse ears' on the corners.
- Turn the part cooling fan off or very low for the first 2-3 layers.
- Raise the bed temperature slightly and keep AC or fan airflow away from the printer.
- Rotate large flat models slightly or add a chamfer to the bottom edges.
🐘
Bottom layers bulging out (Elephant's Foot)
The very bottom of the model flares outward.
Bottom layers bulging out (Elephant's Foot)
The very bottom of the model flares outward.
How to fix
- Raise the Z-offset slightly: the nozzle is squashing the first layer too much.
- Try lowering the bed temperature by 5-10°C.
- Set 'Elephant foot compensation' to 0.1-0.2 mm in your slicer.
- Reduce the first layer flow or line width a little.
〰️
Gaps between first layer lines
First layer lines don't join together; you see gaps or round, thread-like lines.
Gaps between first layer lines
First layer lines don't join together; you see gaps or round, thread-like lines.
How to fix
- The nozzle is too far from the bed: lower the Z-offset until the lines are slightly flattened.
- Run bed leveling / auto bed mesh again, with the bed already heated.
- Set the first layer line width to 110-120%.
- If one side looks fine and the other doesn't, the bed is tilted: check the leveling knobs.
🔪
Rough first layer / nozzle scraping the bed
The first layer shows a wavy pattern, ridges or a thin transparent layer.
Rough first layer / nozzle scraping the bed
The first layer shows a wavy pattern, ridges or a thin transparent layer.
How to fix
- The nozzle is too close: raise the Z-offset slightly (in 0.02-0.05 mm steps).
- Keep the first layer height at 0.2-0.25 mm, not too thin.
- If there's old plastic or debris on the bed, clean it with a scraper.
🍝
Print turned into spaghetti mid-way
The print came off the bed or broke, and the nozzle kept extruding into the air.
Print turned into spaghetti mid-way
The print came off the bed or broke, and the nozzle kept extruding into the air.
How to fix
- Apply all the bed adhesion fixes (clean bed, Z-offset, brim).
- Use supports or a brim for tall, thin models, and slow down.
- Turn on Z-hop in your slicer so the nozzle doesn't hit curled-up areas.
- Check that overhangs have supports underneath.
- If possible, turn on a camera or spaghetti detection.
🕸️
Thin hairs between parts (Stringing)
Spider-web-like strings appear between parts of the model.
Thin hairs between parts (Stringing)
Spider-web-like strings appear between parts of the model.
How to fix
- Increase retraction distance and speed a little in your slicer (direct drive: 0.5-2 mm, Bowden: 4-6 mm).
- Lower the nozzle temperature by 5-10°C.
- The filament may be wet: dry it before use.
- Increase travel speed and enable 'Avoid crossing walls' / combing.
- Print a retraction tower or temperature tower to find the right settings.
🧱
Not enough plastic coming out (Under-extrusion)
Gaps in walls, a weak mesh-like print, holes in the top surface.
Not enough plastic coming out (Under-extrusion)
Gaps in walls, a weak mesh-like print, holes in the top surface.
How to fix
- Check for a nozzle clog (see the 'Nozzle jam' card below).
- Check the extruder gear for filament dust or slipping, and set the tension correctly.
- The temperature may be too low, especially at high speed: raise it by 5-10°C.
- Check that the filament diameter (1.75 mm) and flow rate are correct in your slicer.
- Is the spool tangled? It should turn freely.
🫧
Too much plastic coming out (Over-extrusion)
Blobs on the surface, oversized dimensions and holes that come out too small.
Too much plastic coming out (Over-extrusion)
Blobs on the surface, oversized dimensions and holes that come out too small.
How to fix
- Print a flow rate (extrusion multiplier) calibration and reduce it by 2-5%.
- Make sure the filament diameter in your slicer isn't accidentally set to something other than 1.75.
- Calibrate the extruder e-steps / rotation distance.
- Try lowering the temperature slightly.
🚫
Nozzle jam / no filament coming out
The extruder clicks and nothing, or only a very thin line, comes out of the nozzle.
Nozzle jam / no filament coming out
The extruder clicks and nothing, or only a very thin line, comes out of the nozzle.
How to fix
- Heat the nozzle and gently push the filament by hand: if some comes out, the clog is partial.
- Do a 'cold pull': heat the nozzle to 220-250°C, cool it to 90-100°C, then pull the filament out.
- Clean it from above with the cleaning needle that came with your nozzle.
- If the nozzle is old or worn, replace it. It's one of the cheapest and most reliable fixes.
⚙️
Extruder clicking / knocking
The extruder motor makes a clicking sound and the gear leaves marks on the filament.
Extruder clicking / knocking
The extruder motor makes a clicking sound and the gear leaves marks on the filament.
How to fix
- The temperature is too low for your print speed or flow: raise the temperature or slow down.
- There may be a partial clog: do a cold pull.
- If the extruder tension is too tight, it grinds the filament: loosen it slightly.
- If the nozzle is too close on the first layer, plastic can't come out either: check the Z-offset.
🌡️
Jams partway through a print (Heat creep)
The print starts fine, then extrusion stops after 30-60 minutes.
Jams partway through a print (Heat creep)
The print starts fine, then extrusion stops after 30-60 minutes.
How to fix
- Check that the hotend heatsink fan is running and clean.
- If you're printing PLA in a closed enclosure, open the door or lid.
- Reduce retraction distance; too much retraction pulls hot plastic upward.
- On a Bowden printer, confirm the PTFE tube is seated properly all the way to the nozzle.
💧
Wet filament (popping, bubbles, rough surface)
Popping sounds and steam while printing, small holes in the surface and lots of stringing.
Wet filament (popping, bubbles, rough surface)
Popping sounds and steam while printing, small holes in the surface and lots of stringing.
How to fix
- Dry the filament: PLA 45-55°C, PETG 60-65°C, TPU 50-55°C, Nylon 70-80°C, for 4-8 hours.
- Use a filament dryer or an oven (carefully, at the right temperature).
- Store open spools in an airtight box with silica gel.
- Feed directly from a dry box while printing, especially Nylon and TPU.
👻
Echoes near edges (Ghosting / Ringing)
Wave-like echo lines appear on walls after sharp corners and text.
Echoes near edges (Ghosting / Ringing)
Wave-like echo lines appear on walls after sharp corners and text.
How to fix
- Lower acceleration and jerk / square corner velocity.
- If your printer has input shaping / vibration calibration, run it.
- Check the tension of the X and Y belts.
- Place the printer on a solid, stable table; add rubber feet underneath.
↔️
Layers shifted (Layer Shifting)
Half the print is fine, then the upper part is shifted left or right.
Layers shifted (Layer Shifting)
Half the print is fine, then the upper part is shifted left or right.
How to fix
- Check the X and Y belts: neither too loose nor too tight.
- Tighten the grub screws on the motor pulleys.
- Lower print speed and acceleration; the motor is skipping steps.
- Is the nozzle hitting a curled (warped) area? Turn on Z-hop.
- If the motor driver is very hot, check its cooling.
📏
Uneven layer lines (Z-banding / Wobble)
A repeating band or wave pattern shows up on the walls.
Uneven layer lines (Z-banding / Wobble)
A repeating band or wave pattern shows up on the walls.
How to fix
- Clean the Z lead screw and apply a little grease; check the coupler.
- Use your printer's 'magic number' layer heights (multiples of the motor's full step, such as 0.2, 0.12 or 0.28 mm on common printers).
- If the bed or nozzle temperature is fluctuating, run a PID tune.
- Make sure eccentric nuts / wheels are neither too tight nor too loose.
🧩
Layers splitting apart (Delamination)
The print breaks between layers or shows cracks.
Layers splitting apart (Delamination)
The print breaks between layers or shows cracks.
How to fix
- Raise the nozzle temperature by 5-10°C so layers bond better.
- For ABS/ASA, turn the cooling fan way down and use an enclosure.
- Slow down and increase the wall count.
- Dry the filament; wet filament makes weak layers.
🛏️
Holes or bumps on the top surface (Pillowing)
Small holes or pillow-like bumps appear on the top surface.
Holes or bumps on the top surface (Pillowing)
Small holes or pillow-like bumps appear on the top surface.
How to fix
- Add more top layers: at least a 0.8-1 mm thick top shell (4-5 layers at 0.2 mm).
- Increase infill to 15-20% so the top layer has support.
- For PLA, run the cooling fan at 100% on top layers.
- Turn on 'Ironing' for a smooth finish.
🌉
Sagging overhangs and bridges
Parts printed in mid-air droop, come out rough or break.
Sagging overhangs and bridges
Parts printed in mid-air droop, come out rough or break.
How to fix
- For PLA, run the part cooling fan at 100%.
- Add supports for areas angled more than 45-50°.
- Tune the bridge speed and bridge flow settings in your slicer.
- Rotate the model to reduce overhangs; lower the temperature slightly.
🔘
Bumps on the surface (Blobs & Zits)
Small bumps on the walls, or marks in a straight vertical line (the seam).
Bumps on the surface (Blobs & Zits)
Small bumps on the walls, or marks in a straight vertical line (the seam).
How to fix
- Set the seam position to 'Aligned' or 'Rear' so the marks are hidden at the back.
- Tune retraction and 'Wipe' / coasting settings.
- Calibrate pressure advance / linear advance.
- Check for over-extrusion; reduce flow slightly.
🪜
Supports won't come off / leave marks
Supports fuse to the model, or the surface gets damaged when you remove them.
Supports won't come off / leave marks
Supports fuse to the model, or the surface gets damaged when you remove them.
How to fix
- Set the support Z-distance equal to one layer height (e.g. 0.2 mm).
- Turn on support interface layers and space the interface pattern out a little.
- Try organic / tree supports; they touch the model in fewer places.
- Change the model's orientation so it needs fewer supports in the first place.
🔥
Temperature fluctuating / Thermal error
The nozzle temperature swings up and down, or you get a 'thermal runaway / heating failed' error.
Temperature fluctuating / Thermal error
The nozzle temperature swings up and down, or you get a 'thermal runaway / heating failed' error.
How to fix
- Stop the print immediately, switch the power off and inspect. This is a safety feature; never disable it.
- Run a PID tune for the hotend and the bed.
- Check whether the thermistor or heater wires are loose or broken.
- Fit a silicone sock on the heater block so fan airflow doesn't drop the temperature.
Safety first: Switch the printer OFF and let the nozzle cool down before touching the hotend, wiring or board. The nozzle gets hotter than 200°C.